LOCTITE EA 956

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite EA 956 AERO EPOXY ADHESIVE

Main features

  • 1,000 psi Lap Shear
  • Room-Temperature or Accelerated Heat Cure
  • Low-Viscosity Adhesive Application

Product Description

LOCTITE® EA 956 AERO Epoxy Paste Adhesive is a two-component, amber epoxy adhesive formulated for structural bonding and repair applications requiring elevated-temperature strength. Its low-viscosity mixed consistency supports application by laminating, injection and coating. The adhesive can be cured at room temperature over 5 to 7 days or processed using an accelerated thermal cure for small mixed quantities. When cured for 1 hour at 200°F/93°C, it retains 1,000 psi (6.9 MPa) tensile lap shear strength at 300°F/149°C under ASTM D1002 testing on chromic-acid-etched 2024-T3 AlClad aluminum.

Key features

  • Elevated-temperature bond strength: Retains 1,000 psi (6.9 MPa) tensile lap shear strength at 300°F/149°C after a 1-hour cure at 200°F/93°C.
  • Room-temperature or accelerated cure: Supports a 5-to-7-day cure at 77°F/25°C, with accelerated thermal curing available for small masses.
  • Low-viscosity two-component system: The mixed adhesive has a viscosity of 162 poise at 77°F, supporting repair processes such as injection, laminating and coating.

Applications / Suitable for

  • Repair bonding applications
  • Laminating
  • Adhesive injection
  • Coating applications

Technical Specifications

Physical Properties
Viscosity (Part A)
35,000 mPa.s
Viscosity (Part B)
3,000 mPa.s
General Properties
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:58

Additional Information

Technical properties

As-supplied / before-processing properties

Component, mixed-material, storage and processing data for the uncured two-component adhesive.

Property Part A Part B Mixed Method / condition
Product type Two-component epoxy paste adhesive Requires mixing before application
Color Amber Amber Amber As supplied / mixed
Viscosity at 77°F 350 poise 20 poise 162 poise Brookfield HBT; Part A: spindle 4 at 20 rpm; Part B: spindle 1 at 20 rpm; mixed: spindle 3 at 20 rpm
Viscosity at 25°C 35 Pa·s 3 Pa·s — Brookfield HBT; Part A: spindle 4 at 2.1 rad/s; Part B: spindle 1 at 2.1 rad/s
Density 1.22 g/ml 0.96 g/ml 1.15 g/ml As supplied / mixed
Mix ratio by weight 100 58 100:58 Part A:Part B; volume measurement is not recommended for structural applications unless precautions ensure the correct ratio
Pot life >30 minutes 450 g mass at 77°F/25°C; ASTM D2471 in a water bath
Recommended component temperature before mixing Close to room temperature, 77°F/25°C Separate-component temperature is not otherwise stated as critical
Maximum mixed quantity Do not exceed 250 g Larger quantities may generate dangerous heat buildup and uncontrolled decomposition
Handling-strength cure 6 hours at 77°F/25°C Time to achieve tensile lap shear >500 psi (3.4 MPa)
Handling-strength cure 20 minutes at 140°F/60°C Time to achieve tensile lap shear >500 psi (3.4 MPa)
Handling-strength cure 3 minutes at 185°F/85°C Time to achieve tensile lap shear >500 psi (3.4 MPa)
Handling-strength cure 1 minute at 250°F/121°C Time to achieve tensile lap shear >500 psi (3.4 MPa)
Room-temperature cure 5 to 7 days at 77°F/25°C Stated cure for normal performance
Accelerated complete cure 1 hour at 200°F/93°C For small masses only; accelerated cures are stated up to 200°F/93°C
Shelf life below 40°F/4°C 1 year 1 year — Component shelf life
Shelf life below 77°F/25°C 3 months 1 year — Component shelf life
Shelf life below 90°F/32°C 1 month 1 year — Component shelf life
Technical properties

After-processing / final-state properties

Typical cured adhesive and bonded-joint properties. Values remain specific to the stated cure, specimen, substrate, preparation, test temperature and test method.

Property Value Cure / test condition Method / specimen
Tensile lap shear strength at -67°F/-55°C 1,780 psi (12.3 MPa) Cured 5 days at 77°F/25°C ASTM D1002; 2024-T3 AlClad aluminum, chromic-acid etched
Tensile lap shear strength at -67°F/-55°C 2,400 psi (16.5 MPa) Cured 1 hour at 200°F/93°C ASTM D1002; 2024-T3 AlClad aluminum, chromic-acid etched
Tensile lap shear strength at 77°F/25°C 2,300 psi (15.8 MPa) Cured 5 days at 77°F/25°C ASTM D1002; 2024-T3 AlClad aluminum, chromic-acid etched
Tensile lap shear strength at 77°F/25°C 2,250 psi (15.5 MPa) Cured 1 hour at 180°F/82°C ASTM D1002; 2024-T3 AlClad aluminum, chromic-acid etched
Tensile lap shear strength at 77°F/25°C 2,500 psi (17.2 MPa) Cured 1 hour at 200°F/93°C ASTM D1002; 2024-T3 AlClad aluminum, chromic-acid etched
Tensile lap shear strength at 300°F/149°C 1,000 psi (6.9 MPa) Cured 1 hour at 200°F/93°C ASTM D1002; 2024-T3 AlClad aluminum, chromic-acid etched
Tensile lap shear strength at 400°F/204°C 300 psi (2.1 MPa) Cured 1 hour at 180°F/82°C ASTM D1002; 2024-T3 AlClad aluminum, chromic-acid etched
Tensile lap shear strength at 400°F/204°C 300 psi (2.1 MPa) Cured 1 hour at 200°F/93°C ASTM D1002; 2024-T3 AlClad aluminum, chromic-acid etched
Defined service temperature 300°F (149°C) Cured 1 hour at 200°F/93°C Temperature at which the adhesive retains 1,000 psi (6.9 MPa) under ASTM D1002
Tensile strength at 77°F/25°C 6,900 psi (47.5 MPa) Cured 2 hours at 200°F/93°C ASTM D638; 0.125 in/3.18 mm casting
Tensile strength at 77°F/25°C 5,800 psi (40.0 MPa) Cured 7 days at 77°F/25°C ASTM D638; 0.125 in/3.18 mm casting
Tensile modulus at 77°F/25°C 360 ksi (2,483 MPa) Cured 2 hours at 200°F/93°C ASTM D638; 0.125 in/3.18 mm casting
Tensile modulus at 77°F/25°C 370 ksi (2,552 MPa) Cured 7 days at 77°F/25°C ASTM D638; 0.125 in/3.18 mm casting
Elongation at break at 77°F/25°C 2.54% Cured 2 hours at 200°F/93°C ASTM D638; 0.125 in/3.18 mm casting
Elongation at break at 77°F/25°C 2.35% Cured 7 days at 77°F/25°C ASTM D638; 0.125 in/3.18 mm casting
Shore D hardness at 77°F/25°C 88 Cured 2 hours at 200°F/93°C Bulk resin casting
Shore D hardness at 77°F/25°C 85 Cured 7 days at 77°F/25°C Bulk resin casting
Glass transition temperature, Tg 253°F (123°C) Cured 2 hours at 200°F/93°C Bulk resin casting; Tg method not stated
Glass transition temperature, Tg 156°F (69°C) Cured 7 days at 77°F/25°C Bulk resin casting; Tg method not stated
Compressive strength at 77°F/25°C 12 ksi (82.8 MPa) Cured 7 days at 77°F/25°C ASTM D695; 0.5 in/12.7 mm casting
Compressive modulus at 77°F/25°C 158 ksi (1,089 MPa) Cured 7 days at 77°F/25°C ASTM D695; 0.5 in/12.7 mm casting
Dielectric constant 3.63 0.1 kHz ASTM D149/D150
Dielectric constant 3.59 1.0 kHz ASTM D149/D150
Dielectric constant 3.46 10.0 kHz ASTM D149/D150
Dissipation factor 0.007 0.1 kHz ASTM D149/D150
Dissipation factor 0.017 1.0 kHz ASTM D149/D150
Dissipation factor 0.028 10.0 kHz ASTM D149/D150
Volume resistivity 8.53 × 1014 ohm-cm Cured bulk material ASTM D149/D150
Surface resistivity 2.43 × 1015 ohm Cured bulk material ASTM D149/D150
Thermal conductivity 4.90 × 10−4 cal/s·cm·°C; 0.205 W/(m·K) Cured bulk material Test method and cure condition not stated

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers