LOCTITE ECCOBOND FP4802

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Loctite Eccobond FP4802

Main features

  • High purity
  • Excellent flow
  • Phenolic encapsulant

Product Description

LOCTITE® ECCOBOND FP4802 is a high purity, liquid, phenolic encapsulant designed for use in applications utilizing lead-free solder. This low warpage product can withstand solder reflow temperatures up to 260°C after being exposed to JEDEC level 2 (85°C/60% RH, 168hours) preconditioning. It was formulated to meet “Green” non-halide objectives of many technical users and for temperature cycling ranges up to -65 to 150°C.

LOCTITE ECCOBOND FP4802 features excellent flow properties allowing the material to penetrate fine pitch wires and deep cavities without entrapping voids. A cavity or potting dam is required for flow control.

LOCTITE ECCOBOND FP4802 is suitable for bare chip protection of a variety of advanced packages, such as Ball Grid Arrays (BGA’s), Chip Scale Packages (CSP’s), Plastic Ball Grid Arrays (PBGA’s), and full arrays on Low Temperature cofired Ceramic (LTCC).

 

Cure Schedule

  • 60minutes @ 120°C plus 120minutes @ 165°C
  • 30minutes @ 125°C plus 90minutes @ 165°C

Do not cure with a ramp rate >10°C/minute.

Product Family

233351

30 CC Syringe - 1049155
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 50 days
CA Shipping in 12 weeks
EU Shipping in 50 days
Packaging
Unit of measure Syringe
Net weight 50 g
Gross weight 71 g
Dimensions 3 x 11.9 x 4.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
8 hours
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.76
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
50 °C
Other Properties
MSL Level
MSL 2
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
80,000 mPa.s

Additional Information

LOCTITE ECCOBOND FP4803 is now about to be introduced into the European market. The FP 4803 has been developed for high-volume automotive camera modules and passed all required tests. It claims all the features of 4802 plus a much lower CTE.