3M SJ3540
Harmonization Code : 3926909790 |
Main features
- Black, interlocking mushroom-shaped heads (250 stem density per square inch)
- Mates with Type 170, Type 250 or Type 400 stem densities
- Strong fastener secures with an audible snap, verifying closure
Product Description
3M™ Dual Lock™ Reclosable Fasteners SJ3540 is a high-performance reclosable fastening system designed with a synthetic rubber-based adhesive on the back of a durable black polypropylene strip. Featuring interlocking mushroom-shaped stems, these fasteners provide strong, reliable attachment with the ability to open and close repeatedly. They are engineered for bonding to a wide range of substrates, including low surface energy materials.
Product Key Features
- Mushroom-shaped stems interlock securely for strong fastening with repeated opening and closing
- Available in 250 stems per square inch for varying strength and engagement levels
- Provides excellent initial tack, especially on low surface energy surfaces
- Polypropylene backing ensures long-lasting performance
- Can replace traditional fasteners such as screws, bolts, or snaps in many applications
- Pressure-sensitive adhesive allows quick installation without special tools
Applications
- Attaching panels, covers, and access doors
- Mounting lightweight components and assemblies
- Securing signage, displays, and decorative elements
- Applications requiring frequent removal and reattachment
- Bonding to plastics and other low surface energy materials
- General industrial and commercial fastening solutions
Packaging
Please select Width, Length, Thickness and Color.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Adhesive Layer
Synthetic rubber
A layer that is applied to one surface or both to bind items together and resist their separation